Publication:
Experimental Investigation of the Effect of Specially Manufactured Blank (SMB) Materials on Deep Drawing

dc.authorscopusid57793359600
dc.authorscopusid10939545300
dc.authorscopusid35345218800
dc.authorwosidKöklü, Uğur/Aaq-1387-2020
dc.contributor.authorDagtekin, Emrah
dc.contributor.authorGavas, Muammer
dc.contributor.authorKoklu, Ugur
dc.contributor.authorIDKoklu, Ugur/0000-0002-9205-9768
dc.date.accessioned2025-12-11T01:04:36Z
dc.date.issued2023
dc.departmentOndokuz Mayıs Üniversitesien_US
dc.department-temp[Dagtekin, Emrah] Ondokuz Mayis Univ, Yesilyurt Demir Celik Vocat High Sch, Samsun, Turkey; [Gavas, Muammer] Dumlupinar Univ, Dept Mfg Engn, Kutahya, Turkey; [Koklu, Ugur] Karamanoglu Mehmetbey Univ, Dept Mech Engn, Karaman, Turkeyen_US
dc.descriptionKoklu, Ugur/0000-0002-9205-9768;en_US
dc.description.abstractDeep drawing, one of the sheet metal forming processes, has a large area of use in industry. In the deep drawing, sheets having a fixed thickness are usually deep drawn. In general, there are some limitations, which prevent the part from being drawn at the desired depth, in the deep-drawing processes. Some of these consist of the increase in the sheet thickness towards the end of the part, being exposed to ironing, increasing wrinkles, exposure of the material to deformation hardening, and as a result, the fractures occur in the drawn part. Many special methods have been developed to increase the drawing height. One of them is to use blanks having machined edges. In the present study, the edges of the blank material were thinned by using the turning process at certain angles to avoid the above-mentioned negative effects. In this study, Al-1050 aluminum alloy with a thickness of 2 mm and machined edges of 1 degrees, 2 degrees, 3 degrees, and 4 degrees were used. The results were compared with the unmachined blanks. The highest drawing height was obtained with the blank having a 1 degrees machined edge and 95 mm diameter. In addition, the power (approximately 7-31%) needed for deep drawing and material weight were reduced with the help of the deep-drawing process applied by using a specially manufactured blank.en_US
dc.description.woscitationindexScience Citation Index Expanded
dc.identifier.doi10.1177/09544089221112379
dc.identifier.endpage1309en_US
dc.identifier.issn0954-4089
dc.identifier.issn2041-3009
dc.identifier.issue4en_US
dc.identifier.scopus2-s2.0-85133845613
dc.identifier.scopusqualityQ2
dc.identifier.startpage1300en_US
dc.identifier.urihttps://doi.org/10.1177/09544089221112379
dc.identifier.urihttps://hdl.handle.net/20.500.12712/41158
dc.identifier.volume237en_US
dc.identifier.wosWOS:000822086200001
dc.identifier.wosqualityQ2
dc.language.isoenen_US
dc.publisherSage Publications Ltden_US
dc.relation.ispartofProceedings of the Institution of Mechanical Engineers Part E: Journal of Process Mechanical Engineeringen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectSpecially Manufactured Blanken_US
dc.subjectAngle Machined Blanken_US
dc.subjectDeep Drawingen_US
dc.subjectDrawing Heighten_US
dc.titleExperimental Investigation of the Effect of Specially Manufactured Blank (SMB) Materials on Deep Drawingen_US