dc.department-temp[Çoruh] Semra, Department of Environmental Engineering, Ondokuz Mayis Üniversitesi, Samsun, Turkey; [Ergun] Osman Nuri, Department of Environmental Engineering, Ondokuz Mayis Üniversitesi, Samsun, Turkeyen_US
dc.description.abstractCopper flotation waste from copper production using a pyrometallurgical process contains toxic metals such as Cu, Zn, Co and Pb. Because of the presence of trace amounts of these highly toxic metals, copper flotation waste contributes to environmental pollution. In this study, the leaching characteristics of copper flotation waste from the Black Sea Copper Works in Samsun, Turkey have been investigated before and after vitrification. Samples obtained from the factory were subjected to toxicity tests such as the extraction procedure toxicity test (EP Tox), the toxicity characteristic leaching procedure (TCLP) and the "method A" extraction procedure of the American Society of Testing and Materials. The leaching tests showed that the content of some elements in the waste before vitrification exceed the regulatory limits and cannot be disposed of in the present form. Therefore, a stabilization or inertization treatment is necessary prior to disposal. Vitrification was found to stabilize heavy metals in the copper flotation waste succesfully and leaching of these metals was largely reduced. Therefore, vitrification can be an acceptable method for disposal of copper flotation waste. © 2006 Elsevier Ltd. All rights reserved.en_US
dc.identifier.doi10.1016/j.jenvman.2005.11.006
dc.identifier.endpage338en_US
dc.identifier.issn0301-4797
dc.identifier.issn1095-8630
dc.identifier.issue4en_US
dc.identifier.pmid16730115
dc.identifier.scopus2-s2.0-33750017845
dc.identifier.scopusqualityQ1
dc.identifier.startpage333en_US
dc.identifier.urihttps://doi.org/10.1016/j.jenvman.2005.11.006
dc.identifier.urihttps://hdl.handle.net/20.500.12712/20322
dc.identifier.volume81en_US
dc.identifier.wosWOS:000241923600003
dc.identifier.wosqualityQ1
dc.language.isoenen_US
dc.publisherAcademic Pressen_US
dc.relation.ispartofJournal of Environmental Managementen_US
dc.relation.journalJournal of Environmental Managementen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectCopper Flotation Wasteen_US
dc.subjectMetals Leachabilityen_US
dc.subjectToxicity Testsen_US
dc.subjectVitrificationen_US
dc.titleLeaching Characteristics of Copper Flotation Waste before and after Vitrificationen_US
dc.typeArticleen_US
dspace.entity.typePublication

Files