Publication: Cyclic Fatigue Resistance of XP-Endo Shaper, K3XF, and ProTaper Gold Nickel-Titanium Instruments
| dc.authorscopusid | 56471565700 | |
| dc.authorscopusid | 22934205900 | |
| dc.authorscopusid | 42561320300 | |
| dc.authorscopusid | 35784439500 | |
| dc.contributor.author | Keskin, C. | |
| dc.contributor.author | Inan, U. | |
| dc.contributor.author | Güler, D.H. | |
| dc.contributor.author | Kalyoncuoǧlu, E. | |
| dc.date.accessioned | 2020-06-21T13:10:56Z | |
| dc.date.available | 2020-06-21T13:10:56Z | |
| dc.date.issued | 2018 | |
| dc.department | Ondokuz Mayıs Üniversitesi | en_US |
| dc.department-temp | [Keskin] Cangül, Department of Endodontics, Ondokuz Mayis Üniversitesi, Samsun, Turkey; [Inan] Uǧur, Department of Endodontics, Ondokuz Mayis Üniversitesi, Samsun, Turkey; [Güler] Duygu H., Department of Endodontics, Ondokuz Mayis Üniversitesi, Samsun, Turkey; [Kalyoncuoǧlu] Elif, Department of Endodontics, Ondokuz Mayis Üniversitesi, Samsun, Turkey | en_US |
| dc.description.abstract | Introduction: The aim of this study was to compare the cyclic fatigue resistance of the ProTaper Gold (PTG; Dentsply Maillefer, Ballaigues, Switzerland), K3XF (SybronEndo, Orange, CA), and XP-endo Shaper (FKG Dentaire, La Chaux-de-Fond, Switzerland) nickel-titanium rotary instruments at intracanal temperatures. Methods: Eighteen XP-endo Shaper (30.01), 18 K3XF (30.04), and 18 PTG F3 (30.09v) instruments were used to test the cyclic fatigue resistance at an intracanal temperature of 35° ± 2°C. The instruments were tested in a metal block that simulated a canal curvature angle of 60° and a curvature or radius of 5 mm. All instruments were operated until fracture occurred, and then the number of cycles to failure was calculated. The lengths of fractured fragments were measured with a digital caliper. The data were analyzed statistically using 1-way analysis of variance and the Tukey post hoc test with significance set at P <.05. Results: The XP-endo Shaper instruments showed a significantly higher number of cycles to fracture than the K3XF and PTG instruments (P <.05). There was no difference between the PTG and K3XF instruments (P >.05). Conclusions: The XP-endo Shaper instruments exhibited greater cyclic fatigue resistance compared with the other instruments at the intracanal temperature. © 2018 American Association of Endodontists | en_US |
| dc.identifier.doi | 10.1016/j.joen.2018.04.005 | |
| dc.identifier.endpage | 1167 | en_US |
| dc.identifier.issn | 0099-2399 | |
| dc.identifier.issn | 1878-3554 | |
| dc.identifier.issue | 7 | en_US |
| dc.identifier.pmid | 29866409 | |
| dc.identifier.scopus | 2-s2.0-85048718024 | |
| dc.identifier.scopusquality | Q1 | |
| dc.identifier.startpage | 1164 | en_US |
| dc.identifier.uri | https://doi.org/10.1016/j.joen.2018.04.005 | |
| dc.identifier.volume | 44 | en_US |
| dc.identifier.wos | WOS:000437818800016 | |
| dc.identifier.wosquality | Q1 | |
| dc.language.iso | en | en_US |
| dc.publisher | Elsevier Inc. usjcs@elsevier.com | en_US |
| dc.relation.ispartof | Journal of Endodontics | en_US |
| dc.relation.journal | Journal of Endodontics | en_US |
| dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
| dc.rights | info:eu-repo/semantics/closedAccess | en_US |
| dc.subject | Intracanal Temperature | en_US |
| dc.subject | Nickel-Titanium | en_US |
| dc.subject | Static Cyclic Fatigue Device | en_US |
| dc.title | Cyclic Fatigue Resistance of XP-Endo Shaper, K3XF, and ProTaper Gold Nickel-Titanium Instruments | en_US |
| dc.type | Article | en_US |
| dspace.entity.type | Publication |