Publication:
Evaluation of Bond Strength of Self-Etching Adhesives Having Different pH on Primary and Permanent Teeth Dentin

dc.authorscopusid56019933100
dc.authorscopusid8723440500
dc.authorscopusid56020494600
dc.authorscopusid56019408400
dc.authorscopusid24923690900
dc.contributor.authorOzmen, B.
dc.contributor.authorKoyutürk, A.E.
dc.contributor.authorTokay, U.
dc.contributor.authorCortcu, M.
dc.contributor.authorSari, M.E.
dc.date.accessioned2020-06-21T13:51:15Z
dc.date.available2020-06-21T13:51:15Z
dc.date.issued2015
dc.departmentOndokuz Mayıs Üniversitesien_US
dc.department-temp[Ozmen] Bilal, Department of Pediatric Dentistry, Ondokuz Mayis Üniversitesi, Samsun, Turkey; [Koyutürk] Alp Erdin, Department of Pediatric Dentistry, Ondokuz Mayis Üniversitesi, Samsun, Turkey; [Tokay] Uğur, Department of Pediatric Dentistry, Tishk International University, Erbil, Erbil, Iraq; [Cortcu] Murat, Department of Pediatric Dentistry, Ondokuz Mayis Üniversitesi, Samsun, Turkey; [Sari] Mustafa Erhan, Department of Pediatric Dentistry, Ondokuz Mayis Üniversitesi, Samsun, Turkeyen_US
dc.description.abstractPurpose: The purpose of this in vitro study was to evaluate the dentin shear bond strength of 4 self-etching adhesives having a different pH on primary and permanent teeth dentin. Methods: The occlusal enamel was removed from 60 freshly extracted third molar and 60 primary second molar human teeth, which were randomly separated into 4 groups (n = 15). Four adhesive systems were applied: G-Bond (GC Corporation, Tokyo, Japan, pH: 1.5), Futura Bond M (Voco, Cuxhaver, Germany, pH: 1.4), Adper Prompt L-Pop (3M/ESPE, St Paul, MN, USA, pH: 0.8), and Clearfil S3 Bond (Kuraray Medical, Tokyo, Japan, pH: 2.7) according to the manufacturer’s instructions. After the application of dentin bonding agents, a composite resin material (Z250 Restorative A2, 3M ESPE, St. Paul, MN, USA) for permanent teeth and a compomer resin material (Dyract Extra A2, Dentsply, Konstanz, Germany) for primary teeth was applied onto the prepared dentin surfaces. The data were obtained by using a universal test machine at a crosshead speed of 1 mm/min. Results: The mean values were compared using Tukey’s multiple comparison test. Although there was no difference between adhesives on the permanent teeth, Clearfil S3 adhesive showed higher bond (18.07 ± 0.58 MPa) (P<0.05). Lower bond strength values were obtained from primary teeth and especially G-Bond adhesive (9.36 ± 0.48 MPa) (P<0.05). Conclusions: Self-etching adhesives with different pH and solvent types can be used successfully for permanent teeth dentin but adhesives with low pH did not provide greater shear bond strength values. © 2015 Wichtig Publishing.en_US
dc.identifier.doi10.5301/jabfm.5000234
dc.identifier.endpagee279en_US
dc.identifier.issn2280-8000
dc.identifier.issue3en_US
dc.identifier.pmid26391869
dc.identifier.scopus2-s2.0-84944584398
dc.identifier.scopusqualityQ3
dc.identifier.startpagee274en_US
dc.identifier.urihttps://doi.org/10.5301/jabfm.5000234
dc.identifier.volume13en_US
dc.identifier.wosWOS:000367158000012
dc.identifier.wosqualityQ2
dc.language.isoenen_US
dc.publisherWichtig Publishing Srlen_US
dc.relation.ispartofJournal of Applied Biomaterials & Functional Materialsen_US
dc.relation.journalJournal of Applied Biomaterials & Functional Materialsen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectAggressivenessen_US
dc.subjectDental Adhesivesen_US
dc.subjectDentinen_US
dc.subjectShear Strengthen_US
dc.titleEvaluation of Bond Strength of Self-Etching Adhesives Having Different pH on Primary and Permanent Teeth Dentinen_US
dc.typeArticleen_US
dspace.entity.typePublication

Files