Publication:
Thermokinetic Analysis and Product Characterization of Medium Density Fiberboard Pyrolysis

Loading...
Thumbnail Image

Date

Journal Title

Journal ISSN

Volume Title

Publisher

Research Projects

Organizational Units

Journal Issue

Abstract

This study investigates the pyrolysis of Medium Density Fiberboard (MDF) as a potential waste management solution. Thermal behaviour of MDF was analysed via TG/DSC. The primary decomposition step occurred between 190 °C and 425 °C. Evolved gaseous products over this step were evaluated by a FTIR spectrometer coupled with TGA. Peaks for phenolic, alcohols and aldehydes were detected at the maximum decomposition temperature. Py-GC/MS analysis revealed phenols, ketones and cyclic compounds as the primary non-condensable pyrolysis products. The kinetics of pyrolysis were investigated by the widely applied Distributed Activation Energy Model, resulting in an average activation energy and pre-exponential factor of 127.40 kJ mol−1 and 8.4E+11. The results of this study suggest that pyrolyzing MDF could potentially provide renewable fuels and prevent environmental problems related with MDF disposal. © 2018 Elsevier Ltd

Description

Citation

WoS Q

Q1

Scopus Q

Q1

Source

Bioresource Technology

Volume

258

Issue

Start Page

105

End Page

110

Endorsement

Review

Supplemented By

Referenced By