Basit öğe kaydını göster

dc.contributor.authorYılmaz, Veysel T.
dc.contributor.authorOdabaşoğlu, Mustafa
dc.contributor.authorIcbudak, H
dc.contributor.authorOlmez, H
dc.date.accessioned2020-06-21T11:33:22Z
dc.date.available2020-06-21T11:33:22Z
dc.date.issued1993
dc.identifier.issn0008-8846
dc.identifier.urihttps://doi.org/10.1016/0008-8846(93)90146-Z
dc.identifier.urihttps://hdl.handle.net/20.500.12712/9965
dc.descriptionYilmaz, Veysel/0000-0002-2849-3332;en_US
dc.descriptionWOS: A1993KG80400019en_US
dc.description.abstractCommercial cement superplasticizers(SMF and SNF) were treated with 1M KOH solutions for up to 2.0 days. The chemical changes were characterized by chemical analysis, IR spectroscopy and thermal analysis techniques. After several hours of the preparation, the alkaline solution precipitated SMF and the precipitation ended in 12 days. More than 65% of the initial SMF content was removed from the solution as a white-solid phase. The IR, DTA and TG analysis of the precipitation product of SMF indicated that its chemical and physical properties were altered from that of the original SMF. However, SNF was not degraded by the alkaline solutions.en_US
dc.language.isoengen_US
dc.publisherPergamon-Elsevier Science Ltden_US
dc.relation.isversionof10.1016/0008-8846(93)90146-Zen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.titleThe Degradation of Cement Superplasticizers in A High Alkaline-Solutionen_US
dc.typearticleen_US
dc.contributor.departmentOMÜen_US
dc.identifier.volume23en_US
dc.identifier.issue1en_US
dc.identifier.startpage152en_US
dc.identifier.endpage156en_US
dc.relation.journalCement and Concrete Researchen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US