dc.descriptionPubMed: 28494595en_US
dc.description.abstractAim To evaluate the effects of two different resin coating materials on the clinical performance of a conventional glass ionomer sealant. Subject and methods Permanent first mandibular molars of 60 children aged 6-9 years were sealed with Fuji VII. In each child, G-Coat Plus coating agent was applied to molars on one side and Heliobond coating agent to molars on the opposite side of the mouth. Clinical evaluations were carried out at 1, 6, 12, 18 and 24 months after sealant and coating application. Results At 1, 6, 12, 18 and 24 months after sealant and coating application, total sealant retention rates were 88%, 40%, 19%, 15% and 9% for molars coated with G-Coat Plus, and 93%, 47%, 17%, 15% and 7% for those coated with Heliobond. The differences between the two coating agents were not statistically significant (p>0.05). No incidence of caries was observed in either group during the two-year evaluation period. Statistics: Wilcoxon signed rank test was used to compare differences in retention rates and caries incidence by coating agent. Conclusion Although retention rates of Fuji VII were relatively low and similar for both resin coating agents tested, dental caries were not observed in either group during the 24-month study period. In children with a high risk of caries and partially erupted molars, the use of a glass ionomer sealant with a resin-based coating agent should be encouraged.en_US
dc.language.isoengen_US
dc.publisherAriesdue Srlen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectChilden_US
dc.subjectDecayen_US
dc.subjectGlass ionomer fissure sealanten_US
dc.subjectPreventive dentistryen_US
dc.titleClinical performance of a glass ionomer sealant protected with two different resin-based agents over a 2-year follow-up perioden_US
dc.typereviewen_US
dc.contributor.departmentOMÜen_US
dc.identifier.volume18en_US
dc.identifier.issue1en_US
dc.identifier.startpage10en_US
dc.identifier.endpage14en_US
dc.relation.journalEuropean Journal of Paediatric Dentistryen_US
dc.relation.publicationcategoryDiğeren_US


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster