The effect of layer thickness on the porcelain bond strength of laser-sintered metal frameworks

Date

2019

Author

Kaleli, Necati
Ural, Cagri
Kucukekenci, Ahmet Serkan

Metadata

Show full item record

Abstract

Statement of problem. Laser sintering has become a common manufacturing technique in the fabrication of metal-ceramic restorations. The layer thickness of the sintering process may affect the surface morphology and hence the porcelain bond strength. However, limited information is available on the effect of layer thickness on porcelain bond strength. Purpose. The purpose of this in vitro study was to evaluate the porcelain bond strength of direct metal laser-melted (DMLM) cobalt-chromium (Co-Cr) metal frameworks sintered with 25-mu m and 50-iim layer thicknesses. Material and methods. Thirty metal frameworks (n=10) were fabricated by using the lost-wax technique (group C [control]), DMLM with a 25-mu m layer thickness (group L25), and DMLM with a 50-mu m layer thickness (group L50) according to the International Organization for Standardization (ISO) 9693-1. The surface roughness of 1 metal specimen from each group was analyzed by atomic force microscopy. After porcelain firing, a 3-point bend test was applied to each metal-ceramic specimen as in ISO 9693-1. In addition, 1 metal framework from each group was prepared and examined by scanning electron microscopy to evaluate surface morphology. Data were analyzed statistically by using 1-way analysis of variance and the Tukey honestly significant difference tests (alpha=.05). Results. Group C and group L25 showed significantly higher (P<.001) mean porcelain bond strength values than group L50, and no significant bond strength difference was found between groups C and L25. All groups generally exhibited an adhesive type of failure. Conclusions. The results indicate that layer thickness may affect the porcelain bond strength of DMLM metal frameworks.

Source

Journal of Prosthetic Dentistry

Volume

122

Issue

1

URI

https://doi.org/10.1016/j.prosdent.2018.12.016
https://hdl.handle.net/20.500.12712/10769

Collections

  • Makale Koleksiyonu [14]
  • PubMed İndeksli Yayınlar Koleksiyonu [6144]
  • Scopus İndeksli Yayınlar Koleksiyonu [14046]
  • WoS İndeksli Yayınlar Koleksiyonu [12971]



DSpace software copyright © 2002-2015  DuraSpace
Contact Us | Send Feedback
Theme by 
@mire NV
 

 




| Policy | Guide | Contact |

DSpace@Ondokuz Mayıs

by OpenAIRE

Advanced Search

sherpa/romeo

Browse

All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsTypeLanguageDepartmentCategoryPublisherAccess TypeInstitution AuthorThis CollectionBy Issue DateAuthorsTitlesSubjectsTypeLanguageDepartmentCategoryPublisherAccess TypeInstitution Author

My Account

LoginRegister

Statistics

View Google Analytics Statistics

DSpace software copyright © 2002-2015  DuraSpace
Contact Us | Send Feedback
Theme by 
@mire NV
 

 


|| Policy || Library || Ondokuz University || OAI-PMH ||

Ondokuz Mayıs University, Samsun, Turkey
If you find any errors in content, please contact:

Creative Commons License
Ondokuz University Institutional Repository is licensed under a Creative Commons Attribution-NonCommercial-NoDerivs 4.0 Unported License..

DSpace@Ondokuz Mayıs:


DSpace 6.2

tarafından İdeal DSpace hizmetleri çerçevesinde özelleştirilerek kurulmuştur.